THE DENSITY OF TERNARY BISMUTH–INDIUM–TIN ALLOY OF EUTECTIC COMPOSITION IN THE LIQUID STATE AND IN THE REGION OF MELTING–CRYSTALLIZATION

Rashid A. Khairulin
1. Institute of Thermophysics SB RAS Novosibirsk, Russian Federation
2. Novosibirsk State University Novosibirsk, Russian Federation
Rasul N. Abdullaev
1. Institute of Thermophysics SB RAS Novosibirsk, Russian Federation
2. Novosibirsk State University Novosibirsk, Russian Federation
Sergey V. Stankus
1. Institute of Thermophysics SB RAS Novosibirsk, Russian Federation
stankus@itp.nsc.ru
The material was received by the Editorial Board: 17.08.2012
The temperature dependence of the density of liquid bismuth–indium–tin alloy of eutectic composition (57.20 wt. % Bi; 24.79 wt. % In; 18.01 wt. % Sn) has been investigated using gamma-ray attenuation technique at temperatures from liquidus line to 950 K. The density change during solid–liquid transition has been measured. It has been found that the behavior of the volume properties of the melt is described quite well by the laws of ideal solution.

Keywords:
bismuth–indium–tin eutectic, melt, density, gamma-ray attenuation technique.
УДК 536.41:669.65'872'76

THE DENSITY OF TERNARY BISMUTH–INDIUM–TIN ALLOY OF EUTECTIC COMPOSITION IN THE LIQUID STATE AND IN THE REGION OF MELTING–CRYSTALLIZATION
References: Khairulin R. A., Abdullaev R. N., Stankus S. V. THE DENSITY OF TERNARY BISMUTH–INDIUM–TIN ALLOY OF EUTECTIC COMPOSITION IN THE LIQUID STATE AND IN THE REGION OF MELTING–CRYSTALLIZATION. Vestnik NSU. Series: Physics. 2013, vol. 8, no. 1. P. 104–106 (in Russ.). DOI: 10.54362/1818-7919-2013-8-1-104-106